Izod Impact, Notched 0.716 J/cm

@Thickness 3.17 mm
1.34 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact
High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.716 J/cm

@Thickness 3.17 mm
1.34 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.716 J/cm

@Thickness 3.17 mm
1.34 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact
High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.716 J/cm

@Thickness 3.17 mm
1.34 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled