Mechanical Properties Metric English Comments
Izod Impact, Notched 0.790 J/cm

@Temperature 23.0 °C
1.48 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Izod Impact, Notched 0.790 J/cm

@Temperature -30.0 °C
1.48 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Izod Impact, Notched 0.790 J/cm

@Temperature 23.0 °C
1.48 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Braskem CP 405 XP Injection Molding Polypropylene
Applications: Caps for soft drinks. Information provided by Braskem