Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.471 J/cm

@Thickness 3.17 mm
0.882 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GA-4025 ABS, 25% Glass Filled
Permanent static prevention material with 25% GF reinforcement that can be used in OA device and trayInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.471 J/cm

@Thickness 3.17 mm
0.882 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GA-4025 ABS, 25% Glass Filled
Permanent static prevention material with 25% GF reinforcement that can be used in OA device and trayInformation provided by Samsung Cheil Industries.