Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.970 J/cm @Temperature 23.0 °C |
1.82 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |