Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
1.89 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-115GF-AX00 PC+PBT with Glass Fiber Reinforcement
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.89 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature -20.0 °C |
1.90 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS NAT Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 720 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL2 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 92RK Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS LE WT Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 9129J Rigid PVC, Extrusion Georgia Gulf 9129J is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer which retards color change.Information provided by Georgia GulfGeorgia Gu.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SLX2 MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS X MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |