Mechanical Properties Metric English Comments
Izod Impact, Notched 0.570 J/cm

@Temperature 23.0 °C
1.07 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66
Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.