Polymer Property : Izod Impact, Notched = 1.09 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.580 J/cm

@Temperature -40.0 °C
1.09 ft-lb/in

@Temperature -40.0 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.580 J/cm

@Temperature 23.0 °C
1.09 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar EN067 Copolyester, Natural
Eastar Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, t..