Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.18 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI951 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Izod Impact, Notched | >= 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and .. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR490 ABS, Heat Resistance, Low Emission Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.21 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical 60HR HIPS Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IPM2000 PMMA- ABS Alloy High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.18 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm |
2.20 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |