Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.772 J/cm @Temperature 23.0 °C |
1.45 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Provista NXT Copolymer Resin for Profile Extrusion Applications:Candy packagingCorner guardsDisplays, Fixtures and Point of purchaseFood packagingFurniture guardsIntegrated circuit tubesLighting tubesPlastics for hygiene feminine productsPricing cha.. |