Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.20 - 1.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.25 - 2.81 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |