Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.10 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.10 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF43 IM L BKN 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Izod Impact, Notched | 1.66 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
3.10 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |