Mechanical Properties Metric English Comments
Izod Impact, Notched 1.6667 J/cm

@Thickness 3.20 mm
3.1224 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade
Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali
Izod Impact, Notched 1.6667 J/cm

@Thickness 3.20 mm
3.1224 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade
Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali