Polymer Property : Izod Impact, Notched = 1.70 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.900 - 1.70 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
1.69 - 3.18 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256, ISO 180/4a
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact
Characteristics: high fluidity, high impact