Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.72 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Izod Impact, Notched 0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Izod Impact, Notched 0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Izod Impact, Notched 0.920 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.72 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Izod Impact, Notched 0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GFN1430V PPE+PS
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Izod Impact, Notched 0.920 J/cm

@Temperature -30.0 °C
1.72 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Notched 0.920 J/cm

@Temperature -30.0 °C
1.72 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Notched 0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Izod Impact, Notched 0.920 J/cm

@Temperature -30.0 °C
1.72 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GFN1420V PPE+PS
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Izod Impact, Notched 0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..