Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -29.0 °C |
1.80 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® FG1901 + PA-6 blend (20/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature -30.0 °C |
1.80 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature 23.0 °C |
1.80 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl EM6100F PPE+PS Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel.. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 835 Sheet Extrusion Grade Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex .. |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature -18.0 °C |
1.80 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & gar.. |