Polymer Property : Izod Impact, Notched = 1.98 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.98 J/cm

@Temperature 22.8 °C
3.70 ft-lb/in

@Temperature 73.0 °F
1/2" x 1/8"; ASTM-D256
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade
Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams.
Izod Impact, Notched 1.98 J/cm

@Temperature 23.0 °C
3.71 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp
Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,..
Izod Impact, Notched 1.98 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.70 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Axiall 8264 Rigid PVC, Extrusion
Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. ..