Polymer Property : Izod Impact, Notched = 10.3 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 10.3 J/cm

@Thickness 3.17 mm
19.3 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 10.3 J/cm

@Thickness 3.17 mm
19.3 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.