Mechanical Properties Metric English Comments
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 84110 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by..
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 5.71 J/cm

@Temperature 23.0 °C
10.7 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Izod Impact, Notched 5.70 J/cm

@Temperature 23.0 °C
10.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature -30.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 5.70 J/cm

@Temperature -10.0 °C
10.7 ft-lb/in

@Temperature 14.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East)
XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab..
Izod Impact, Notched >= 5.69 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 10.7 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GP5006B PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Izod Impact, Notched 5.69 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical MA221 ABS, High Impact, Low Gloss
Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 5.69 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 5.69 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 5.71 J/cm

@Thickness 3.17 mm,
Temperature -28.9 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature -20.0 °F
ASTM D-256
Axiall Suprel® 9422 Rigid PVC, Molding
Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with..
Izod Impact, Notched 5.69 J/cm

@Thickness 3.20 mm
10.7 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron BL60 Impact modifier for PVC
Impact modifier for PVC, White powderInformation provided by Bhansali
Izod Impact, Notched 5.70 J/cm

@Temperature 23.0 °C
10.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Izod Impact, Notched 5.69 J/cm

@Thickness 3.20 mm
10.7 ft-lb/in

@Thickness 0.126 in
ASTM D256