Polymer Property : Izod Impact, Notched = 10.8 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 5.77 J/cm

@Temperature -20.0 °C
10.8 ft-lb/in

@Temperature -4.00 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer
High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors. US ..
Izod Impact, Notched 5.75 J/cm

@Temperature 23.0 °C
10.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg..
Izod Impact, Notched 5.75 J/cm

@Temperature 23.0 °C
10.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..