Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.6 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
21.7 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 11.6 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
21.7 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 11.6 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
21.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 8607 Rigid PVC, Extrusion Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |