Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 7.00 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
13.1 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 22.2 °C |
13.1 ft-lb/in @Temperature 72.0 °F |
ASTM D256 |
PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Asia Pacific) Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at lo.. |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Europe-Africa-Middle E.. |