Mechanical Properties Metric English Comments
Izod Impact, Notched 13.2 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
24.8 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 13.2 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
24.8 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Axiall 7803 Rigid PVC, Extrusion High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.