Mechanical Properties Metric English Comments
Izod Impact, Notched 7.26 J/cm

@Temperature 0.000 °C
13.6 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene
Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination ..
Izod Impact, Notched 7.28 J/cm

@Temperature 23.0 °C
13.6 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer
40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 7.26 J/cm

@Temperature 23.0 °C
13.6 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Kraton® G1657 + PA-6 blend (16/4/80)
Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..