Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion LR840 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding MR840 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 7.52 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -40.0 °C |
14.1 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -30.0 °C |
14.1 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 7.53 J/cm @Thickness 3.17 mm, Temperature -17.8 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 0.000 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 7.53 J/cm @Thickness 3.17 mm, Temperature -17.8 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 0.000 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 7.52 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -40.0 °C |
14.1 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
14.1 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
Injection Molded; ASTM D256 |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |