Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.68 J/cm @Temperature 23.0 °C |
18.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPM1944 PC Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Izod Impact, Notched | 9.68 J/cm @Temperature 23.0 °C |
18.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Izod Impact, Notched | 9.68 J/cm @Temperature 23.0 °C |
18.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Izod Impact, Notched | 9.66 J/cm @Temperature 23.0 °C |
18.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |