Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.77 J/cm @Temperature 23.0 °C |
18.3 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1652 + PPE blend (20/80) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |