Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.883 - 1.08 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.65 - 2.02 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |