Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.6471 J/cm

@Thickness 3.20 mm
4.9591 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Izod Impact, Notched 2.6471 J/cm

@Thickness 3.20 mm
4.9591 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali