Mechanical Properties Metric English Comments
Izod Impact, Notched 2.84 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.33 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Izod Impact, Notched 2.84 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
5.33 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.84 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
5.33 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.84 J/cm

@Thickness 6.35 mm
5.33 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.84 J/cm

@Thickness 6.35 mm
5.33 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.84 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
5.33 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.84 J/cm

@Thickness 6.35 mm
5.33 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.84 J/cm

@Thickness 6.35 mm
5.33 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.