Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant Chemical Resistant GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 3.20 mm |
5.5101 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 3.20 mm |
5.5101 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 3.20 mm |
5.5101 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-20P ABS Sheet Extrusion Grade ABS Pipe GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-20P ABS Sheet Extrusion Grade ABS Pipe GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 3.20 mm |
5.5101 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.9412 J/cm @Thickness 6.40 mm |
5.5101 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant Chemical Resistant GradeInformation provided by Bhansali |