Mechanical Properties Metric English Comments
Izod Impact, Notched 2.97 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
5.56 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Kingfa HC-110 Modified ABS
Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.