Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.1 J/cm @Temperature 23.0 °C |
20.8 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1657 + PA-6,6 blend (16/4/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 11.1 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
20.8 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 11.1 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
20.8 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 11.1 J/cm @Thickness 6.35 mm |
20.8 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall Vynaprene 7907 Rigid PVC, Extrusion Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre.. |