Mechanical Properties Metric English Comments
Izod Impact, Notched 11.48 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
21.51 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
notch
Kraton® G1657 + PA-6 blend (8/12/80)
Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..