Izod Impact, Notched 11.75 J/cm

@Thickness 3.20 mm
22.01 ft-lb/in

@Thickness 0.126 in
reverse notched; ASTM D 256
SABIC Innovative Plastics Ultem 1010K PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.