Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 13.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
24.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 13.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
24.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 13.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
24.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |