Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 3.24 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.24 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
6.06 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS650 ABS
Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.24 J/cm

@Temperature 23.0 °C
6.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H1000PWI High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weathering, reduce heat conductivity to waterRecommended Applications: Above ground pipes, double wall pipesInforma..
Izod Impact, Notched 3.24 J/cm

@Temperature 23.0 °C
6.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LA50 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.24 J/cm

@Temperature -30.0 °C
6.06 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LA50 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.24 J/cm

@Temperature 23.0 °C
6.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LA60 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.24 J/cm

@Temperature -30.0 °C
6.06 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LA60 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.24 J/cm

@Temperature 23.0 °C
6.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LB40 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.24 J/cm

@Temperature -30.0 °C
6.06 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LB40 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Copyright © lookpolymers.com All Rights Reserved