Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.7647 J/cm @Thickness 3.20 mm |
3.3060 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |