Mechanical Properties Metric English Comments
Izod Impact, Notched 1.80 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.37 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LI-943 ASA Resin  (discontinued **)
Heat resistance, Excellent weather resistance, Well balanced mechanical properties, Superior chemical resistance, Good thermal aging stability, Good moldability and processability, Applications incl..
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Izod Impact, Notched 1.80 J/cm

@Temperature -30.0 °C
3.37 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific)
LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 1.80 J/cm

@Temperature -18.0 °C
3.37 ft-lb/in

@Temperature -0.400 °F
ASTM Test
Styrolution Terluran® HI-10 ABS
Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 1.25%); ASTM-D256
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.80 J/cm

@Temperature -40.0 °C
3.37 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 2.9%); ASTM-D256
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 1.0%); ASTM-D256
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D256
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE 0425 GFS Acrylonitrile Butadiene Styrene, 13% Glass Filled
ABS with 13% short glass fiberExcellent mechanical and thermal propertiesInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.80 J/cm

@Temperature 0.000 °C
3.37 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.80 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
3.37 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256, ISO 180/4a
EPICHEM Epiryl B PPO Polyphenylene oxide
Izod Impact, Notched 1.80 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
3.37 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256, ISO 180/4a
EPICHEM Epiryl PPO V0 Polyphenylene oxide
Characteristics: self-extinguishing V0 at 1,6 mm