Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HR-527A Modified ABS Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HG193S ABS, High Flow, Chemical Resistance Feature: Injection Molding, High Flow, Chemical ResistanceApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.96 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 3.67 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CA-7009 PA/PPE, Antistatic Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
3.67 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VS-0800 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® CA-7009 PA/PPE, Antistatic Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Temperature -20.0 °C |
3.67 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PWI High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, reduce heat conductivity to waterRecommended Applications: Above ground pipes, double wall pipesInforma.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm |
3.67 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 100Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm |
3.67 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm |
3.67 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |