Mechanical Properties Metric English Comments
Izod Impact, Notched 2.03 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
3.80 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa HF-618 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Izod Impact, Notched 2.03 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Izod Impact, Notched 2.03 J/cm

@Temperature 23.0 °C
3.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Formosa Plastics Formolene® 6507N Impact Copolymer Polypropylene
Impact Copolymer for Injection Molding Formolene® 6507N is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional stabil..
Izod Impact, Notched 2.03 J/cm

@Temperature 23.0 °C
3.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and..
Izod Impact, Notched 2.03 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
3.80 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
Diamond Polymers ABSPC 7430-1005T ABS/PC Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 2.03 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.80 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 2.03 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.80 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
Axiall 7803 Rigid PVC, Extrusion High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 2.03 J/cm

@Temperature 23.0 °C
3.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 360A4861301 Propionate Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..