Polymer Property : Izod Impact, Notched = 3.8570 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.0588 J/cm

@Thickness 3.20 mm
3.8570 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali
Izod Impact, Notched 2.0588 J/cm

@Thickness 3.20 mm
3.8570 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali