Izod Impact, Notched 2.47 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.63 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa HF-626 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.