Polymer Property : Izod Impact, Notched = 4.89 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.61 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.89 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Kingfa H-12 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Izod Impact, Notched 2.61 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.89 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa HP-126 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.