Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.13 J/cm @Temperature 23.0 °C |
9.60 ft-lb/in @Temperature 73.4 °F |
1/8'' notched bar, partial failure, (Room temperature); ASTM D256 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |