Polymer Property : Izod Impact, Notched = 5.68 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.03 J/cm

@Temperature -40.0 °C
5.68 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS
Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.