Izod Impact, Notched 3.11 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.83 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa FW-650 Flame Retardant ABS
Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd.