Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.10 J/cm @Temperature 23.0 °C |
11.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |