Izod Impact, Notched 3.48 J/cm

@Temperature 23.0 °C
6.52 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 572E3720012 Cellulose Acetate Butyrate, Clear, Trsp
Applications:FilmsProfilesSheetProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a wa..