Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.52 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
6.60 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 3.52 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
6.60 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |