Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.5294 J/cm @Thickness 3.20 mm |
6.6120 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.5294 J/cm @Thickness 3.20 mm |
6.6120 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.5294 J/cm @Thickness 6.40 mm |
6.6120 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.5294 J/cm @Thickness 6.40 mm |
6.6120 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.5294 J/cm @Thickness 6.40 mm |
6.6120 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.5294 J/cm @Thickness 6.40 mm |
6.6120 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |